Prior art keywords
arc welding
ceramic
contact tip
contact
ceramic coating
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP60057222A
Other languages
English (en)
Japanese (ja)
Other versions
JPS61217567A (ja
Inventor
Tadao Amasaka
Misao Iwata
Kazumi Fujikawa
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Toyota Motor Corp
Original Assignee
Toyota Motor Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Toyota Motor Corp filed Critical Toyota Motor Corp
Priority to JP60057222A priority Critical patent/JPS61217567A/ja
Publication of JPS61217567A publication Critical patent/JPS61217567A/ja
Publication of JPH0140910B2 publication Critical patent/JPH0140910B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Arc Welding In General (AREA)
  • Coating By Spraying Or Casting (AREA)
JP60057222A 1985-03-20 1985-03-20 ア−ク溶接用コンタクトチツプのセラミツク被覆方法 Granted JPS61217567A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP60057222A JPS61217567A (ja) 1985-03-20 1985-03-20 ア−ク溶接用コンタクトチツプのセラミツク被覆方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP60057222A JPS61217567A (ja) 1985-03-20 1985-03-20 ア−ク溶接用コンタクトチツプのセラミツク被覆方法

Publications (2)

Publication Number Publication Date
JPS61217567A JPS61217567A (ja) 1986-09-27
JPH0140910B2 true JPH0140910B2 (en]) 1989-09-01

Family

ID=13049499

Family Applications (1)

Application Number Title Priority Date Filing Date
JP60057222A Granted JPS61217567A (ja) 1985-03-20 1985-03-20 ア−ク溶接用コンタクトチツプのセラミツク被覆方法

Country Status (1)

Country Link
JP (1) JPS61217567A (en])

Families Citing this family (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102123815B (zh) * 2008-08-13 2016-04-13 米亚基株式会社 电弧焊接用焊枪

Also Published As

Publication number Publication date
JPS61217567A (ja) 1986-09-27

Similar Documents

Publication Publication Date Title
JP6477867B2 (ja) 被覆金型およびその製造方法
JP6717450B2 (ja) 軽金属基板の二層鉄コーティング
US3031330A (en) Method of bonding an outer coating of one metal to a base surface of aluminum or the like
CN115190916B (zh) 具有抗磨损性和防腐蚀性的制动盘及其生产方法
KR20060039922A (ko) 코팅
US3868235A (en) Process for applying hard carbide particles upon a substrate
JPS6117912B2 (en])
JPH0255502B2 (en])
JP3076768B2 (ja) 薄膜形成装置用部材の製造方法
JPH0140910B2 (en])
CN107904547A (zh) 一种钛合金耐磨耐高温涂层的制备方法
JP3029405B2 (ja) 耐摩耗コーティング部品の製造方法
JPH0371943B2 (en])
JP2993773B2 (ja) 電気めっきライン用コンダクタロ−ル及びその製造方法
CN117568767A (zh) 一种刀具涂层及其制备方法和应用
JP3403460B2 (ja) 非酸化物系セラミック溶射皮膜を有する炭素材料の製造方法
CN109321860A (zh) 一种工件耐磨涂层及其喷涂方法
JP2000345313A (ja) 繰り返し熱衝撃及び摺動摩耗を受けるロール胴部基材表面の耐熱性、耐食性、耐摩耗性を向上させた連続鋳造に用いるロール製造法
KR100439411B1 (ko) 허스롤의 용사코팅방법
CN112226723B (zh) 一种大气氛围下含铝合金涂层的制备方法
JPH0413854A (ja) 耐摩耗・耐食性溶融亜鉛浴中ロール
JPH0757904B2 (ja) 熱処理炉用ロールおよびその製造法
JP2736525B2 (ja) 溶射方法
JP3448784B2 (ja) 表面に皮膜形成材としての電極と基材とを接触させ、アーク放電により溶着させる放電被覆処理法により形成した耐熱耐焼付性皮膜を有する圧延工程用ロール類
KR100820987B1 (ko) 내마모성 코팅 재료를 기계 부품에 피복하는 방법 및 그에의해 형성되는 기계 부품

Legal Events

Date Code Title Description
LAPS Cancellation because of no payment of annual fees